ROTOMOLDING Grade LLDPE Agens Materiam Compositionem Pulvis spumans, LLD484P est gradus spumae LLDPE pulvis rotoplastici mutationis cum spumoso ratione 4. Temperatus incipiens circiter 150℃ est, et temperatus optimus spumosus est circiter 180℃.
ROTOMOLDING Grade LLDPE Agens Materiam Compositionem Pulvis spumans, LLD484P est gradus spumae LLDPE pulvis rotoplastici mutationis cum spumoso ratione 4. Temperatus incipiens circiter 150℃ est, et temperatus optimus spumosus est circiter 180℃.
Formae |
Commercial: active |
Availability |
AS |
Additivum |
HS |
Features |
|
usus |
Implens |
Agency Ratings |
ROHS |
Packaging |
20Kg / packaging |
Fasciae vita |
I annis a die productionis |
Datasheet | Typical Pretio | Unitas | Test Methodi |
Corporalis | |||
Density | - | g/cm3 | ISO1183 |
Mole Density | 0.250 | g/cm3 | ISO60 |
Index solve (190℃,2.16Kg) | 3.2 | g/10min | ISO1133 |
Arida O Rate | 24 | s/100g | ARM |
E.S.C.R. | - | h | ASTM D1693 |
Liquescens punctum | 119 | ℃ | ISO11357 |
Mechanica | |||
Distrahentes confortamini ad cede | 6 | MPa | ISO527 |
Distractatio distrahentes ad cede | 50 | % | ISO527 |
Flexuralis Modulus | 210 | MPa | ISO178 |
impulsum virtus | - | J/mm | ARM |
Duritia, Shore D | - | D | ISO868 |
Scelerisque | |||
Declinatio Caloris (0.45MPa) | - | ℃ | ISO75 |
Vicat molliens Point | - | ℃ | ISO306 |
Bridness Temperature | - | ℃ | ISO974 |
Canus | |||
Oxidation Induction Time | 20 | min | ISO11357 |
UV Rating | - | h | ASTM 2565 |
Other | |||
Superficies Resistentia | - | Ω | IEC60093 |
Flamma retardant | - | Gradus | UL-94 |
Hic dux data est propria notae producti notitiae, et non potest adhiberi ut indices certae qualitatis.